- Interactive modules
- 4 Engineering Tools
- Hydraulic coolants
- Water & PG25 / PG50
- EM & roughness span
- 50 Hz – 30 GHz
- Execution & privacy
- 100% Client-Side
Interactive Engineering Workbench
Values update live locally; copy briefs, share exact URL states, or sync directly into Tool 04.
Tool 01 · Material & manufacturing route screening
Copper AM Alloy & Process Selector
Evaluate 532 nm green-laser LPBF (pure copper, aged CuCrZr/CW106C, GRCop-42) against conventional CNC machining, skiving, or brazing with 5-axis feasibility scoring.
Screening output
Strong LPBF candidateRecommended manufacturing route
532 nm Green-Laser LPBF + CNC Finishing
Candidate copper alloy
Pure Copper (primary) or Aged CuCrZr if thin pressure walls govern
Cu-ETP / Cu-OF / C10100–C11000 powder class
- Published IACS Band
- ~92–100% IACS (post-processed screening)
- Thermal Conductivity
- ~370–395 W/m·K
- Yield Strength Band
- ~60–110 MPa YS (as-built / stress-relieved)
- Service Ceiling
- Typical continuous duty <= 150 °C
5-axis engineering screening fit (relative index)
Key DfAM & acceptance gates
- • Verify minimum channel diameter (>= 0.8–1.0 mm target), bend radius, and accessible powder-exit ports.
- • Allocate CNC stock on mating flats, sealing O-ring grooves, and soft pure-copper mounting interfaces.
- • Specify working pressure, hydrostatic proof ratio, hold time, and helium leak criteria in the RFQ.
COPPER 3DP — Alloy & Process Screening Brief Component: Liquid cold plate / microchannel plate Screened Route: 532 nm Green-Laser LPBF + CNC Finishing (Strong LPBF candidate) Candidate Alloy: Pure Copper (primary) or Aged CuCrZr if thin pressure walls govern Geometry: Internal / curved channels or monolith manifold Operating Temp: Up to 150 °C Initial Volume: 1–5 pcs engineering prototype Screening Scores: AM Fit 92/100 · Conductivity 96/100 · Mech 38/100 · Depowder 66/100 Critical Flags: Pressurized/helium leak boundary Note: Screening reference only; confirm DfAM, witness-coupon state, and final quotation against STEP/drawing.
Screening guidance only—not an unconditional manufacturing or property guarantee. Confirm STEP/CAD with info@szcomo.com .
Tool 02 · Single-phase thermal-hydraulic & DfAM depowdering screen
Cold Plate & Internal Channel Thermal-Hydraulic Estimator
Estimate coolant flow rate, Reynolds number, straight-tube Darcy-Haaland pressure drop (ΔP), Gnielinski convective HTC (h), copper erosion velocity margin, and LPBF L/D_h depowdering risk.
- Total Flow Rate
- 4.48 L/min
- 0.0758 kg/s
- Straight-Tube ΔP
- 5.11 kPa
- 0.051 bar · P_hyd 0.38 W
- Channel Velocity
- 2.06 m/s
- Laminar (f = 0.032)
- Convective HTC (h)
- 1,098 W/m²K
- 0.0839 K/W (Nu 3.7)
- Reynolds Number
- 2,030
- Laminar ≤ 2300
- LPBF Length Ratio
- 75 : 1
- 108.6 cm² wetted
Comfortable LPBF channel cleaning margin (Dh = 1.60 mm, L/Dh = 75); add ~15–25% allowance above straight-tube ΔP for manifold turns.
COPPER 3DP — Cold Plate & Internal Channel Hydraulic Screening Duty: 1500 W @ ΔT = 5.0 °C · Fluid: PG25 35 °C Geometry: 18 parallel paths × Ø1.60 mm × L 120 mm (L/Dh = 75) · Wall Ra/ε: 15.0 µm Flow & Regime: ṁ = 0.0758 kg/s (4.48 L/min) · v = 2.06 m/s · Re = 2030 (Laminar) Straight-Tube Drop & HTC: ΔP = 5.11 kPa (0.051 bar, P_hyd = 0.38 W) · h = 1098 W/m²K · R_conv = 0.0839 K/W Depowdering Gate: Standard LPBF depowdering window Note: Straight-tube analytical estimate only; manifolds, bends, expansion/contraction losses, and conjugate 3D conduction require CFD/CAD review.
Tool 03 · Electromagnetic screening & surface-roughness AC loss (50 Hz – 30 GHz)
Copper Skin Depth & Hammerstad-Bekkadal Roughness Analyzer
Calculate skin depth (δ = √(ρ / (π f μ0))), 1.6δ–2δ wall windows, smooth surface resistance Rs, and as-built vs polished KSR roughness loss multiplier.
- Skin depth (δ)
- 678.0 µm
- Inductor wall (1.6–2δ)
- 1.08 mm–1.36 mm
- Resistivity ρ(T)
- 1.81 µΩ·cm
- Smooth Rs
- 0.027 mΩ/sq
- As-Built KSR
- 1.000×
- Polished KSR
- 1.000×
- Polishing Loss Gain
- < 1% impact
Induction-heating window (0.15–2 mm): active inductor walls can be tailored near 1.6δ–2δ while balancing coolant pressure walls, bend radii, and internal powder removal.
COPPER 3DP — Skin Depth & Surface-Roughness Screening Frequency: 10 kHz (1.00e+4 Hz) Conductivity Input: 95% IACS @ 20 °C · Temp: 20 °C (α = 0.00393 /°C) · ρ(T) = 1.81 µΩ·cm Skin Depth (δ): 678.0 µm · 1.6δ–2.0δ Wall Window: 1.08 mm–1.36 mm Smooth Surface Resistance Rs: 0.027 mΩ/sq Hammerstad-Bekkadal K_SR: 1.000× (Ra 8.0 µm) vs 1.000× (Ra 0.8 µm) -> ~0.0% roughness-loss margin LPBF Screening Note: Induction-heating window (0.15–2 mm): active inductor walls can be tailored near 1.6δ–2δ while balancing coolant pressure walls, bend radii, and internal powder removal.
Tool 04 · Unified quotation package generator
Copper AM RFQ Scope & Acceptance Builder
Consolidate material state, post-processing, and NDT inspection requirements alongside active screening results from Tools 01–03 into a copyable brief or downloadable CSV.
Generated RFQ brief
COPPER 3DP — Structured Copper AM RFQ Brief 1. Application: Cold plate / liquid cooling block 2. Material Route: Commercially pure copper 3. Quantity Scenario: 1-5 pcs prototype 4. Envelope / Operating Duty: To be shared with CAD / drawing 5. Post-Processing & Finishing: Stress relief / CuCrZr precipitation aging; CNC finish machining (datums, flatness, ports); Internal depowdering & flushing 6. Inspection & Acceptance Scope: CMM dimensional report on machined datums; Hydrostatic proof pressure & helium leak test 7. Requested Response: DFM route check, material/heat-treatment confirmation, and scoped quotation.
Reply within 2 business days · NDA on request · Blank inspection templates in Knowledge Center.
Engineering reference & GEO methodology
Benchmark tables, governing equations, and source boundaries
Every screening calculation on this page uses deterministic physics and bounded reference tables so thermal, RF, and procurement teams share reproducible numbers before submitting CAD.
| Alloy route | Designations | Conductivity band | Thermal k band | Yield strength | Primary RFQ evidence |
|---|---|---|---|---|---|
| Commercially Pure Copper (532 nm LPBF) | Cu-ETP / Cu-OF / C10100–C11000 powder class | ~92–100% IACS (post-processed screening) | ~370–395 W/m·K | ~60–110 MPa YS (as-built / stress-relieved) | Verify finished conductivity via witness coupons; plan CNC stock on clamping & sealing lands. |
| Aged CuCrZr / CuCr1Zr Alloy | EN CW106C / DIN 2.1293 / UNS C18150 | ~75–85% IACS (aged condition) | ~310–350 W/m·K | ~280–360 MPa YS (aged condition) | Lock solution + aging heat treatment before final CNC finish; do not specify as-built unaged state. |
| GRCop-42 Dispersion-Strengthened Alloy | Cu-4Cr-2Nb (Cr2Nb Laves phase) | ~65–75% IACS | ~280–320 W/m·K | Retains strength & creep resistance > 350 °C | Confirm powder lot availability, thermal cycle envelope, and qualification scope before quotation. |
| Frequency | Typical band | Skin depth (δ) | 1.6–2δ wall | K_SR (Ra 8 µm) | LPBF design note |
|---|---|---|---|---|---|
| 50 Hz | Grid / power busbars | 9.35 mm | 14.95 mm–18.69 mm | 1.00× | Bulk cross-section governs; AM earns value via 3D routing or integrated water cooling. |
| 1 kHz | Low-frequency induction | 2.09 mm | 3.34 mm–4.18 mm | 1.00× | Active wall thickness and cooling-passage spacing balance electrical and mechanical load. |
| 10 kHz | Mid-frequency induction | 660.8 µm | 1.06 mm–1.32 mm | 1.00× | Practical LPBF sweet spot for tailored inductor walls with conformal internal cooling. |
| 100 kHz | High-frequency induction | 209.0 µm | 334.4 µm–418.0 µm | 1.00× | Mechanical strength and pressure-boundary wall thickness typically exceed 2δ; watch surface finish. |
| 13.56 MHz | ISM / RF plasma | 17.9 µm | Mechanical wall | 1.26× | As-built LPBF roughness (Ra 8 µm -> K_SR ~1.30×) raises AC losses; review polishing or Ag plating. |
| 10 GHz | X-band waveguides | 0.66 µm | Mechanical wall | 2.00× | Surface roughness (K_SR -> 2.00× ceiling) and Ag/Au plating dominate insertion loss. |
| 30 GHz | Ka-band / mmWave | 0.38 µm | Mechanical wall | 2.00× | Tight internal Ra and aperture tolerances control feasibility; evaluate polishing or split-block hybrid. |
| Coolant fluid | Density ρ | Specific heat c_p | Viscosity μ | Thermal k / Pr | Engineering note |
|---|---|---|---|---|---|
| Deionized Water (25 °C nominal) | 997.0 kg/m³ | 4181 J/kg·K | 0.890 mPa·s | 0.607 W/m·K · Pr 6.13 | Baseline reference; verify corrosion control / plating against wetted copper. |
| Deionized Water (40 °C nominal) | 992.2 kg/m³ | 4179 J/kg·K | 0.653 mPa·s | 0.631 W/m·K · Pr 4.32 | Lower viscosity reduces ΔP; evaluate O-ring, pump cavitation, and plating compatibility. |
| 25% Propylene Glycol / Water (PG25, 35 °C) | 1014.0 kg/m³ | 3960 J/kg·K | 1.650 mPa·s | 0.480 W/m·K · Pr 13.60 | Common data-center CDU fluid; higher viscosity raises laminar-to-turbulent transition. |
| 50% Propylene Glycol / Water (PG50, 35 °C) | 1031.0 kg/m³ | 3560 J/kg·K | 3.850 mPa·s | 0.365 W/m·K · Pr 37.60 | Freeze-protected loop; expect substantially higher pressure drop in narrow channels. |
Electromagnetic & IACS basis
NBS Handbook 100, MIT 6.013 & Hammerstad-Bekkadal
δ = sqrt(ρ(T) / (π · f · µ₀)), ρ₂₀ = 1.7241×10⁻⁸ / (%IACS / 100) Ω·m
K_SR = 1 + (2/π) · atan(1.4 · (R_q / δ)²), R_q ≈ 1.25 · R_a
Annealed copper reference ρ₂₀ and temperature dependence follow NBS Handbook 100; surface-roughness AC penalty follows Hammerstad & Bekkadal (1975) for conductor loss screening.
Thermal-hydraulic correlations
Darcy-Weisbach, Haaland (1983) & Gnielinski (1976)
f_lam = 64 / Re · f_turb = [−1.8 · log₁₀((ε/(3.7·D_h))^1.11 + 6.9/Re)]⁻²
Nu_turb = (f/8)(Re−1000)Pr / [1 + 12.7·sqrt(f/8)·(Pr^(2/3) − 1)]
Haaland provides explicit closure within ~1.5% of Colebrook-White across rough LPBF walls; Gnielinski screens fully developed turbulent convection against a laminar Nu = 3.66 lower bound.
LPBF DfAM & depowdering gates
Minimum channel diameter, L/D_h ratio & velocity limits
Sub-0.8 mm hydraulic diameters and L/D_h > 150 paths elevate trapped copper powder risk and demand flush ports plus industrial CT inspection. Coolant velocities above ~2.5 m/s in bare copper warrant parallel path widening, CuCrZr, or electroless nickel protection.
Validation & quotation boundary
ASME V&V 20 & drawing-level release evidence
Screening calculators evaluate idealized geometry and do not replace 3D conjugate CFD, finite-element stress checks, or witness coupons. Full traceability and acceptance evidence are scoped in the formal project quotation and technical source library.
Next engineering steps
Move from screening calculations to validated copper hardware
Custom Copper Cold Plates
Microchannel cooling plates, CNC sealing lands, optional electroless Ni plating, CT, and helium leak checks.
Review cold plate scopeCuCrZr / CuCr1Zr Alloy Service
EN CW106C / DIN 2.1293 / UNS C18150 aged copper-alloy builds for pressurized blocks, threads, and tooling.
Compare CuCrZr specsThermal Design & Validation
Conjugate CFD architecture screening, topology reconstruction, flow distribution, and test correlation.
Explore validation workflowCopper Induction Coils
Complex 3D inductor profiles with integrated cooling and brazed-free repeatable geometries.
View coil tolerancesRF Waveguides & Vacuum Hardware
Precision RF apertures, surface finishing, Ag/Au plating access, and UHV flange flatness.
Check RF readiness6 Procurement Decision Guides
Close alloy state, port seals, manifold flow balance, and qualification gates before formal PO.
Open decision guidesTools FAQ
How to use these copper 3D printing tools before quoting
Clear engineering boundaries between browser-local screening math and drawing-level quotation evidence.
Do these copper 3D printing tools guarantee finished-part properties or instant pricing?
No. Every output is an engineering screening estimate grounded in textbook physics and published copper AM reference bands. Final thermal/electrical conductivity, minimum achievable channel geometry, tolerances, heat-treatment state, and delivered pricing are confirmed against your CAD, 2D drawing, and acceptance scope in the formal quotation.
What are the assumptions behind the Cold Plate Hydraulic & Depowdering Estimator?
The estimator models steady-state single-phase flow distributed evenly across parallel circular channels of length L and diameter Dh. Mass flow comes from heat load and allowable fluid ΔT; Darcy friction uses 64/Re in laminar flow (Re ≤ 2300) and the explicit Haaland/Colebrook-White approximation in turbulent flow (Re ≥ 4000); convection uses 3.66 in laminar flow and the Gnielinski correlation in turbulent flow. Real manifolds add entrance, bend, and distribution pressure losses that should be verified by CFD.
How does surface roughness affect copper RF waveguides and high-frequency inductors?
When electromagnetic skin depth δ approaches or falls below surface roughness Rq, high-frequency current follows surface peaks and valleys, multiplying resistive losses. Using the Hammerstad-Bekkadal model with representative as-built LPBF Ra (around 6–12 µm) shows why polishing, electroplating (Ag/Au), or hybrid CNC split-blocks matter above ~10 MHz, while grid and 1–10 kHz induction coils are far less sensitive to roughness.
How accurate is the copper skin depth calculator for CuCrZr or elevated temperatures?
The calculator pairs alloy-specific screening resistivity (% IACS at 20 °C) and temperature coefficients (0.00393 /°C for pure copper, ~0.00310 /°C for aged CuCrZr) with the standard skin-depth equation δ = sqrt(ρ / (π f µ0)). Because finished-part resistivity depends on chemistry, solution/aging heat treatment, and operating thermal gradient, confirm final IACS targets with witness coupons on your RFQ.
When does the Alloy & Process Selector recommend CNC, skiving, or brazing instead of LPBF?
When cooling fins are straight and tool-accessible or annual production reaches hundreds of uniform parts without internal conformal passages, CNC machining, skiving, stamping, or vacuum brazing typically delivers lower unit cost. The selector scores geometric AM value and volume economics explicitly so your team avoids paying for additive complexity that does not buy performance.
How do I transfer my calculated screening numbers into a formal quotation?
Open Tool 04 (RFQ Scope & Acceptance Builder) and click "Import active calculator results" to merge your screened route, hydraulic target, and skin-depth parameters into a single brief, or click "Share link" to save a reproducible URL for your team. Then click "Open pre-selected RFQ form" to submit your CAD and paste the brief.